Introduction
Polyurethane Lined composite Steel Pipe is a kind of composite pipe made by special process, which is based on steel pipe and lined with polyurethane material with high wear resistance, high elasticity and high corrosion resistance.Polyurethane composite pipe has excellent wear resistance, acid resistance, alkali resistance, scale resistance, radiation resistance, hydrolysis resistance,aging resistance, high elasticity, mechanical impact resistance and other comprehensive properties.
Product Name:Polyurethane Lined composite Steel Pipe
Matrix: steel pipe
Properties: wear resistance, acid resistance, alkali resistance, knot resistance
Pharacteristics: good water resistance stability, good aging resistance
Main Application
Polyurethane composite steel pipe has excellent wear resistance, acid resistance, alkali resistance, scale resistance, radiation resistance, hydrolysis resistance, high elasticity, mechanical impact resistance and other comprehensive properties.It can be widely used in power, coal, mining, building materials, chemical and other industries to transport pulverized coal, ash, mineral powder, liquid aluminum, mud and other grinding granular materials and corrosive media.
Mining industry: iron ore slurry, mine concentrate, tailings transportation system, mine flotation system closed circulation pipeline, water and sand transportation for gold mining.
Technical parameters
The test items | ordinary polyurethane test result | Nano-modified polyurethane test result | Measurements |
Tensile strength | 15-21MPa | 19-28Mpa | GB528-2008 |
300%set the stretching strength | 8-10Mpa | 11-13MPa | GB528-2008 |
Tensile elongation | 400-500% | 400-500% | GB528-2008 |
Break permanent deformation | 43959 | 43959 | GB528-2008 |
The tear strength | 5Mpa/cm | 6.8Mpa/cm | GB528-2009 |
Shear strengh | 6Mpa/cm2 | 8.1MPa/cm2 | HB-853-1994 |
Avulsion intensity | 7.5Mpa/cm2 | 11MPa/cm2 | GBI689-1994 |
peel stenghth | 1.4Mpa2.5/cm | 2.1Mpa/2.5cm | GBI554-1994 |
Akron abrasion | 0.015cm3/1.61km | 0.008cm3/1.61km | GBI689-1998 |
Low temperature brittleness | -42 | -70 | GBI682-2005 |
Hardness (shawA) | 60-100 | 60-100 | GB531-2004 |
The density | 1.12 | 1.2 | GB533-2009 |